A novel avenue for engineering 2D MXene family via precious metals atomic layer deposition techniques

2 years ago 729
A team of researchers, led by Professor Soo-Hyun Kim in the Graduate School of Semiconductors Materials and Devices Engineering and the Department of Materials Science and Engineering at UNIST has made significant progress in precisely controlling precious metals (Ru, Ir, Pt, Pd) incorporation by atomic layer deposition (ALD).